为了满足纺棉型化纤精梳质量要求,介绍棉型化纤性能、精梳工艺参数设置,通过精梳数学模型计算和设计整体锡林齿数、齿面圆心角和分区数、齿形、纵横向齿密以及顶梳针密等参数,并采用
薛  庆
(金轮针布(江苏)有限公司,江苏 南通  226143)
 
摘要:为了满足纺棉型化纤精梳质量要求,介绍棉型化纤性能、精梳工艺参数设置,通过精梳数学模型计算和设计整体锡林齿数、齿面圆心角和分区数、齿形、纵横向齿密以及顶梳针密等参数,并采用GJX-E-75-TP42型和GJX-E-90-X型精梳整体锡林配用不同齿密顶梳,对棉型涤纶普梳和精梳后纺制的14.6 tex成纱质量指标进行对比。结果表明,GJX-E-75-TP42型整体锡林配套GJD-E-240-P型顶梳,适纺精条指标要求较高及落棉率较低的棉型化纤;GJX-E-90-X型整体锡林配套GJD-E-260-B型顶梳梳理的棉型化纤,成纱质量较高但落棉率略高;在棉型化纤纺纱流程中引入精梳工序,能够提升精梳棉网的清晰度以及纤维的伸直度、平行度和分离度,用户可根据棉型化纤的质量要求进行选配。
关键词:棉型化纤;精梳;整体锡林;顶梳;隔距;梳理度;棉结;杂质;短绒率;落棉率
中图分类号:TS103.82+1      文献标志码:B      文章编号:1001-9634(2018)02-0010-05
 
收稿日期:2017-07-26
作者简介:薛  庆(1969—),男,江苏海门人,高级工程师,主要从事机械设计、梳理器材开发等方面的研究。
网络出版时间:2018-01-02 10:44
http://www.cnki.net/kcms/detail/61.1131.TS.20180102.1044.002.html
 
Design and Configuration of Integrated Combing Cylinderand the Top Comb for Cotton-like Chemical Fiber
XUE Qing
(Geron Card Clothing(Jiangsu)Co.,Ltd.,Nantong 226143,China)
 
Abstract:To meet the quality requirements of combing process of cotton-like chemical fiber,introduction is done to cotton-like chemical fiber regarding the properties,and combing process parameters.Through combing mathematical model calculation and design of tooth number,radius angle and the number of partitions,tooth shape,both crosswise and lengthways density of integrated cylinder and top comb density,equipping the combing integrated cylinders GJX-E-75-TP42 and GJX-E-90-X with different tooth density of top comb,comparison is done to the yarn quality of the cotton-like polyester fiber 14.6 tex both carded and worsted.The results show that the integrated cylinder GJX-E-75-TP42 if configured with top comb GJD-E-240-P is applicable for cotton-like chemical fibers with higher fine index and lower noil rate while integrated cylinder GJX-E-90-X if configured with top comb GJD-E-260-B is applicable for spinning cotton-like chemical fiber,yet with high yarn quality and slight high noil rate.Spinning process of cotton-like chemical fiber if combing process is introduced,can enhance the worsted web clarity and fiber straightness,parallelism and separation,the user can make decision as process required.
Key Words:cotton-like chemical fiber;combing;integrated cylinder;top comb;gauge;carding degree; neps;impurities;short fiber rate;noil rate
 
参考文献:
[1] 周金冠.现代精梳生产工艺与技术[M].北京:中国纺织工业出版社,2006.
[2] 任家智.精梳机对纤维长度的适纺性研究[J].棉纺织技术,2004,32(1):13-16.
[3] 任家智.纺纱工艺学[M].上海:东华大学出版社,2010:61-76.
[4] 任家智.E62型精梳机工艺特性分析[J].棉纺织技术,2005,33(8):15-19.
[5] 赵建伟.合理控制精梳落棉率稳定产品质量的体会[J].棉纺织技术,2010,38(7):27-31.
[6] 刘红艳,任家智,冯清国,等.棉精梳锡林总齿数设计方法的探讨[J].中原工学院学报,2016,27(6):48-51.
[7] Switzerland:Rieter Machine Works Ltd,Werner K.立达纺纱手册(第3册)[Z].

相关热词搜索:锡林 精梳 化纤

上一篇:环锭细纱机导纱板升降机构改进
下一篇:高硬度纳米氮化铬钢领

分享到: 收藏