2022-10-26 08:16:47   来源:   评论:0 点击:

为了有效减少细纱断头,从纱线强力、张力方面分析细纱断头的本质,将原发断头分为细偏支强力弱环断头、卷绕张力断头、慢输张力断头、附入断头4大类;在分析原发断头特点及成因的基础


路红星
(中橡(江苏)胶业科技有限公司,江苏 泰州   225411)
 
摘要:为了有效减少细纱断头,从纱线强力、张力方面分析细纱断头的本质,将原发断头分为细偏支强力弱环断头、卷绕张力断头、慢输张力断头、附入断头4大类;在分析原发断头特点及成因的基础上,提出避免其产生危害的措施。指出:断头的本质是张力与强力矛盾的表现,即断面处强力小于作用在该处的张力,要准确判断、辨证施治、精准预防;控制断头的重点是慢输张力断头和附入断头,减少原发断头就能减少次生断头和断头总量。
关键词:细纱;原发断头;细偏支强力弱环断头;慢输张力断头;附入断头;卷绕张力断头
中图分类号:TS104.2          文献标志码:C          文章编号:1001-9634(2022)04-0057-05
 
收稿日期:2021-11-05
作者简介:路红星(1976—),男,河南辉县人,主要从事胶辊胶圈应用与管理方面的工作。
 
Clarifying the Essence of Broken Ends,Improving Process Management
LU Hongxing
(Zhongxiang (Jiangsu) Rubber Industry Technology Co.,Ltd.,Taizhou 225411,China)
 
Abstract:In order to reduce spinning broken ends effectively,the essence of spinning broken ends is analyzed from the aspects of yarn strength and tension,and the primary broken ends are divided into four categories:thin deviation count strength weak point broken ends,winding tension broken ends,slow feed tension broken ends,and attachment broken ends.On the basis of analyzing the characteristics and causes of broken ends,the measures to avoid its harm are put forward.It is pointed out that the essence of broken ends is the performance of the contradiction between tension and strength,which means that the strength at the cross-section is less than the tension acting on it,so it is necessary to judge accurately,treat dialectically,and prevent accurately.The key point of control of broken ends are slow feed tension broken ends and attachment broken ends,and reducing primary broken ends can reduce secondary broken ends and the total amount of broken ends.
Key Words:spinning; primary broken ends; thin deviation count strength weak point broken ends; slow feed tension broken ends; attachment broken ends; winding tension broken ends
 
参考文献:
[1] 顾菊英.棉纺工艺学:下册[M] .北京:中国纺织出版社,1991.
[2] 路红星.细纱机后、中下罗拉打顿原因及预防[J] .纺织器材,2013,40(2):32-34.
[3] 路红星.纺纱胶辊磨伤探析[J] .纺织器材,2012,39(2):29-31.
[4] 张国梁.国产钢领差距和特殊曲线内跑道设计与加工[J] .纺织器材,2012,39(2):1-5.
[5] 路红星.甄选纺纱器材专件的思考[J] .纺织器材,2016,43(6):49-51.
[6] 陆宗源.钢丝圈变速运动对纱线断头的影响[J] .纺织器材,2017,44(2):6-12.
[7] 路红星.提高和稳定牵伸力的技术探讨[J] .棉纺织技术,2019,47(11):70-74.
 


相关热词搜索:细纱 原发断头

上一篇:方便装卸绒卷的条干仪纱架
下一篇:条筒圈存容量扩增技术的现状与创新

分享到: 收藏